The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent tracking resistance in electronics and extreme low water absorption of HFFR cable compounds, where vinylsilane modified APYRAL® products are almost indispensable.APYRAL ® can be used as a flame retardant filler in ThermosetsElastomersThermoplasticsCable CompoundsTechnical Rubber CompoundsPressed and cast Plastic PartsThermal Insulation FoamsGlass-fiber reinforced plastics
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Brightness 91 %

@Wavelength 457 nm
91 %

@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 45 %
45 %
ml/100 g
Loss On Ignition 35.0 %

@Temperature 105 - 1000 °C
35.0 %

@Temperature 221 - 1830 °F
Particle Size 1.3 µm
1.3 µm
Median Grain Diameter
Specific Surface Area 6.0 m²/g
6.0 m²/g
BET
Mechanical Properties Metric English Comments
Hardness, Mohs 3
3
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
Component Elements Properties Metric English Comments
Fe2O3 0.010 %
0.010 %
Na2O 0.40 %
0.40 %
SiO2 0.30 %
0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 20000 ohm-cm
20000 ohm-cm
Descriptive Properties Value Comments
Al(OH)3 wt % 98.5
Mechanical Properties as Additive Elongation at break: 210 %
Tensile Strength: 16 Mpa
HFFR-EVA cable compound
Sieve Analysis (%) 0.05
> 45 µm