Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.3 µm | 1.3 µm | Median particle diameter |
Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film streng.. |
|||
Particle Size | 1.3 µm | 1.3 µm | Median Grain Diameter |
Nabaltec APYRAL® 60 VS1 Al(OH)3 The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent.. |
|||
Particle Size | 1.3 - 2.0 µm | 1.3 - 2.0 µm | Average |
H.C. Starck Grade B Titanium Carbonitride Hard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 1.3 - 1.9 µm | 1.3 - 1.9 µm | Average |
H.C. Starck Grade B Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 1.3 µm | 1.3 µm | Median Grain Diameter |
Nabaltec APYRAL® 40CD Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |