NanoAmor 90%, OD: 1-2 nm OH Functionalized Single-Walled Carbon Nanotubes

Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 90%, OD: 1-2 nm OH Functionalized Single-Walled Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and shieldingEnergy conversionLithium-battery anodesHydrogen storageNanotube composites (by filling or coating);Nanoprobes for STM, AFM, and EFM tips, nanolithography, nanoelectrodes, drug delivery, sensorsReinforcements in compositesSupercapacitorInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
average diameter
Specific Surface Area 400 m²/g
400 m²/g
Descriptive Properties Value Comments
Color black
Content of -OH wt% 1 to 7
Length (um) 5-30
Mole fraction of surface carbon atoms 21 to 26
Purity (vol% carbon nanotubes), min 95
Purity (vol% single-walled nanotubes), min 90