Polymer Property : Particle Size = 0.0010 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
from HRTEM
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
NanoAmor 60% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
average diameter
NanoAmor 60%, OD: 1-2 nm COOH Functionalized Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
average diameter
NanoAmor 60%, OD: 1-2 nm OH Functionalized Single-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
NanoAmor 90% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
average diameter
NanoAmor 90%, OD: 1-2 nm OH Functionalized Single-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
average diameter
NanoAmor 90%, OD: 1-2 nm COOH Functionalized Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0020 µm
0.0010 - 0.0020 µm
wall thickness
NanoAmor 94%, OD/WT/L: 20-50/1-2 nm/0.5-2 um Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.0030 µm
0.0010 - 0.0030 µm
core diameter
NanoAmor 95%, OD/ID: 3-20/1-3 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Particle Size 0.0010 - 0.040 µm
0.0010 - 0.040 µm
American Elements Silver Nanoparticles
General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp..
Particle Size 0.0010 - 0.030 µm
0.0010 - 0.030 µm
American Elements Copper Oxide Nanopowder
General DescriptionCopper Oxide (CuO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Copper Oxide Particles are typically 1-30 nanometers (nm)..