Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes

Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and shieldingEnergy conversionLithium-battery anodesHydrogen storageNanotube composites (by filling or coating);Nanoprobes for STM, AFM, and EFM tips, nanolithography, nanoelectrodes, drug delivery, sensorsReinforcements in compositesSupercapacitorInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
true density
Apparent Bulk Density 0.170 g/cc
0.00614 lb/in³
Particle Size 0.0050 - 0.010 µm
0.0050 - 0.010 µm
inside diameter
0.010 - 0.020 µm
0.010 - 0.020 µm
outside diameter
Specific Surface Area 200 m²/g
200 m²/g
Descriptive Properties Value Comments
Color black
Length (um) 0.5-2
Purity (vol% carbon nanotubes), min 95