Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95% 10-20 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | <= 0.010 µm | <= 0.010 µm | outside diameter |
NanoAmor 95%, OD/ID: ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD: 10-20 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | outside diameter |
NanoAmor 95%, OD: 10-20 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Aluminum Nitride Nanoparticles General DescriptionAluminum Nitride (AlN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Aluminum Nitride Particles are typically 10 - 100 nanometers (nm).. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Boron Nitride Nanoparticles General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Calcium Carbonate Nanoparticles General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Dysprosium Oxide Nanopowder General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Particle Size | 0.010 - 0.045 µm | 0.010 - 0.045 µm | |
American Elements Europium Nanoparticles General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Lanthanum Oxide Nanopowder General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanomete.. |
|||
Particle Size | 0.010 - 0.050 µm | 0.010 - 0.050 µm | |
American Elements Lithium Nanoparticles General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Nickel Oxide Nanopowder General DescriptionNickel Oxide (NiO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Nickel Oxide Particles are typically 10-30 nanometers (nm.. |
|||
Particle Size | 0.010 - 0.040 µm | 0.010 - 0.040 µm | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Particle Size | 0.010 - 0.020 µm | 0.010 - 0.020 µm | |
American Elements Niobium Nanoparticles General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Palladium Nanoparticles General DescriptionPalladium (Pd) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Palladium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Particle Size | 0.010 - 0.045 µm | 0.010 - 0.045 µm | |
American Elements Praseodymium Nanoparticles General DescriptionPraseodymium (Pr) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Praseodymium Particles are typically 10 - 45 nanometers (nm) wit.. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Samarium Oxide Nanopowder General DescriptionSM-MITE powders and dispersions are inorganic samarium-oxide nanoparticles. SM-MITE-A products are uncoated and hydrophilic. SM-MITE-O products are coated with an organic silane (.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nanotubes General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers .. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Silicon Nitride Nanoparticles General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w.. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Terbium Nanoparticles General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific.. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Terbium Oxide Nanopowder General DescriptionTB-MITE powders and dispersions are inorganic terbium-oxide nanoparticles. TB-MITE-A products are uncoated and hydrophilic. TB-MITE-O products are coated with an organic silane (1.. |
|||
Particle Size | 0.010 - 0.10 µm | 0.010 - 0.10 µm | |
American Elements Titanium Nitride Nanoparticles General DescriptionTitanium Nitride (TiN) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Titanium Nitride Particles are typically 10 - 100 nanometer.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Vanadium Oxide Nanopowder General DescriptionVanadium Oxide (VO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Vanadium Oxide Particles are typically 10-30 nanometers .. |
|||
Particle Size | 0.010 - 0.080 µm | 0.010 - 0.080 µm | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Chromium Oxide Nanopowder General DescriptionChromium Oxide (CrO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Chromium Oxide Particles are typically 10-30 nanometers.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Cobalt Oxide Nanopowder General DescriptionCobalt Oxide (CoO) Nanoparticles, nanodots or nanopowder are white spherical high surface area metal particles. Nanoscale Cobalt Oxide Particles are typically 10-30 nanometers (nm.. |