Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NanoScale NanoActive® Zinc Oxide

Category Ceramic , Oxide
Manufacturer NanoScale
Trade Name NanoActive®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoScale NanoActive® Zinc Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduced particle sizes (the volume weighted mean is below 0.3 µm).Applications: Applications include catalysts and catalyst supports, cosmetic and skin care market, paints and coatings, solar cells, transparent UV resistant coatings, and varistors.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Density 5.60 g/cc
0.202 lb/in³
Loss On Ignition <= 4.0 %
<= 4.0 %
Particle Size 4.0 µm
4.0 µm
mean aggregate size
Specific Surface Area >= 70 m²/g
>= 70 m²/g
BET
Pore Size 0.0170 microns
0.000669 mil
Average Diameter
Component Elements Properties Metric English Comments
Zinc, Zn >= 99 %
>= 99 %
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Appearance / Color Off-White Powder
Crystallite Size = 10 nm
Minimum Total Pore Volume cc/g 0.2
Users viewing this material also viewed the following: