Nanocyl EPOCYL™ NC E1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for non-Solvent Formulation Purposes

Category Polymer , Thermoset , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Nanocyl
Trade Name EPOCYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl EPOCYL™ NC E1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for non-Solvent Formulation Purposes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EPOCYL™ NC E1MY-02 is a Mater Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enhance electrical conductivity of high Tg epoxy-based formulations. Special features include easy integration and great flexibility in processing. Dilution factor has to be calculated accordingly to the desired level of conductivity.ApplicationsElectrostatic discharge (ESD) coatings, linings (tanks, rollers, ...) and compositesConductive primersResistive inksAdhesivesBenefitsLimited impact on base resin mechanical and thermo-mechanical propertiesEase of formulationOther information available upon request to NanocylCuring agents EPOCYL™ NCE1MY-02 based formulations can be cured or cross-linked with different types of curing agents which could be decided accordingly to the desired processing conditions and the properties of the final composite like any conventional tetrafunctional based formulations.
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.18 g/cc
1.15 - 1.18 g/cc
Viscosity 5000 - 35000 cP

@Temperature 60.0 °C
5000 - 35000 cP

@Temperature 140 °F
Measured with parallel plate in dynamic mode ar 10 rad/s and a strain of 1%.
235000 - 345000 cP

@Temperature 25.0 °C
235000 - 345000 cP

@Temperature 77.0 °F
Measured with parallel plate in dynamic mode ar 10 rads/s and a strain of 1%.
Electrical Properties Metric English Comments
Volume Resistivity 900 ohm-cm
900 ohm-cm
70 parts per 100 of NC E1MY-02 in the final compound
8000 ohm-cm
8000 ohm-cm
35 parts per 100 of NC E1MY-02 in the final compound
10000 ohm-cm
10000 ohm-cm
12 parts per 100 of NC E1MY-02 in the final compound
40000 ohm-cm
40000 ohm-cm
12 parts per 100 of NC E1MY-02 in the final compound
Descriptive Properties Value Comments
Aspect Paste, black (Master Batch)
Epoxy Equivalent 112.2 - 119.5 g/eq
Epoxy Value 8.36 - 8.91 eq/kg
Storage Temperature 5°C