Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 900 ohm-cm | 900 ohm-cm | 70 parts per 100 of NC E1MY-02 in the final compound |
Nanocyl EPOCYL™ NC E1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for non-Solvent Formulation Purposes EPOCYL™ NC E1MY-02 is a Mater Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enhance.. |