Material Notes:
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours at 73°F; ASTM D570
Water Absorption at Saturation 0.35 %
0.35 %
73°F; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.56 MPa
7913 psi
chs 2 in/min; ASTM D638
Elongation at Break 233 %
233 %
ASTM D638
Flexural Modulus 2.15 GPa
312 ksi
Tangent (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched NB
NB
Reverse Notched 0.125 in bar; ASTM D256
Gardner Impact >= 36.2 J

@Temperature -18.0 °C
>= 26.7 ft-lb

@Temperature -0.400 °F
ASTM D5420
>= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D-5420
>= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003