Material Notes:
Description: Natural NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Water Absorption 8.0 %
8.0 %
Saturation; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 134 MPa
19400 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Flexural Strength 192 MPa
27800 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
1/8 in specimen; ASTM D256
Thermal Properties Metric English Comments
Melting Point 218 °C
425 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 191 °C
375 °F
0.125 in bar; ASTM D648