Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 20-3401 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12 |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF10 A1 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF20 L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Aclo Accutech ABS ABS833G20L Glass Reinforced |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFIPP 2030 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |