NextGen Adhesives G907-24 Structural Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives G907-24 Structural Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC G907-24 is a medium viscosity and near transparent adhesive system that is specifically formulated for structural applications requiring excellent wetting, mechanical strength and chemical resistance.Advantages and Applications: The NGAC G907-24 is easily mixed and cured at room temperature and provides excellent adhesion to glass, ceramic, metal and plastic. It is highly chemically resistant with superior mechanical strength.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Solids Content 100 %
100 %
Viscosity 12000 cP
12000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 20 min
20 min
Descriptive Properties Value Comments
Color Transparent
Mix Ratio by Weight (R/H) 100/25