This low carbon steel has good case hardening properties. Although not classed as a screw machine steel, at times it may be specified. This is an excellent steel for bending and cold forming, with good brazing and welding properties.Information provided by Niagra LaSalle Corporation
Mechanical Properties Metric English Comments
Hardness, Brinell 126
126
Tensile Strength 441 MPa
64000 psi
Tensile Strength, Yield 372 MPa
54000 psi
Elongation at Break >= 15 %
>= 15 %
2"
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.15 - 0.20 %
0.15 - 0.20 %
Iron, Fe 97.65 - 99.1 %
97.65 - 99.1 %
as balance
Manganese, Mn 0.60 - 0.90 %
0.60 - 0.90 %
Phosphorous, P <= 0.40 %
<= 0.40 %
Silicon, Si 0.15 - 0.35 %
0.15 - 0.35 %
Sulfur, S <= 0.50 %
<= 0.50 %