Material Notes:
This is basic screw machine steel. The grade is used as a standard of comparison for machinability (1212 is rated as 100%). It machines easily, provides good surface finish and has good brazing properties. This steel is difficult to weld and not suitable for case hardening. Generally used where mechanical properties can be sacrificed for machinability.Information provided by Niagra LaSalle Corporation
Mechanical Properties Metric English Comments
Hardness, Brinell 167
167
Tensile Strength 538 MPa
78000 psi
Tensile Strength, Yield 414 MPa
60000 psi
Elongation at Break >= 10 %
>= 10 %
2"
Reduction of Area 35 %
35 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.13 %
<= 0.13 %
Iron, Fe 98.52 - 99.07 %
98.52 - 99.07 %
as balance
Manganese, Mn 0.70 - 1.0 %
0.70 - 1.0 %
Phosphorous, P 0.070 - 0.12 %
0.070 - 0.12 %
Sulfur, S 0.16 - 0.23 %
0.16 - 0.23 %