Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0190 cm/cm
0.0190 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 60.0 %
60.0 %
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Unnotched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 249 - 260 °C
480 - 500 °F
ASTM D789
Descriptive Properties Value Comments
Color Natural