Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
SABIC PP 506P Polypropylene Homopolymer for Raffia Applications Product Description: PP 506P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speeds and low deniersLow tap.. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF5020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Temperature | 235 - 260 °C | 455 - 500 °F | ISO 294 |
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | Extruder |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LATI Latiblend 3675 G/10 ABS/PBT, 10% Glass Fiber Reinforced Blend based on Acrylonitrile-Butadiene-Styrene copolymer (ABS) / Polybutylene Terephthalate (PBT). Glass fibers. Good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Polymer Mass Temp |
Borealis Daplen™ EE115T TPO Compound Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
TPI Porene® KU900 Super High Heat ABS INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Injection Molding |
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir.. |