Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Melt Flow 6.00 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.00 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D123
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Unnotched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
269 °F
ASTM D648
Vicat Softening Point 157 °C
314 °F
ASTM D789
Descriptive Properties Value Comments
Color Black