Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 93.1 MPa | 13500 psi | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Oxford Polymers PC 46 Unfilled Polycarbonate for Blow and Extrusion Molding Unfilled Polycarbonate for Blow and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Niche Polymer PCM6BK PC Information provided by Niche Polymer |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
PolyOne Edgetek® AS-50GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
PolyOne Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Fiberfil® J-60/20/E4 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 93.1 MPa | 13500 psi | |
SGL Carbon Group EK 3105 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Techmer ES Luriblend® PA6 GL15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TL20 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Low Friction and Good Wear ResistanceUL File Number: E157318TPCI# 9740101Information provided by TP Compos.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Chase Plastics CP Pryme® PC100R Polycarbonate Molding Resin, Mold Release Information provided by Chase Plastics. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Chase Plastics CP Pryme® PC100RUV Polycarbonate, Mold Release, UV Stabilized Information provided by Chase Plastics. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Entec Hylex® P1025L1 HB Polycarbonate Available in North America Features: General Purpose Agency Ratings: FDA 21 CFR 177.1580 RoHS Compliant Form: Pellets Information provided by Entec |