Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 H-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 H-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Water Absorption 1.4 - 2.4 %
1.4 - 2.4 %
ISO 62
Water Absorption at Saturation 5.0 - 7.0 %
5.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0050 - 0.014 cm/cm
0.0050 - 0.014 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 180 MPa
26100 psi
ISO 2039-1
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527
Flexural Strength 230 MPa
33400 psi
ISO 178
Flexural Modulus 7.70 GPa
1120 ksi
ISO 178
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
DIN 53453
NB
NB
ISO 179/1eU
3.60 J/cm²

@Temperature -40.0 °C
17.1 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
DIN 53453
0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V
550 V
CTI 100; IEC 112