Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-GV30 Nylon 6.6, std. viscosity for injection molding, 30% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL A63 H-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Nilit FRIANYL B63 GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CLG902 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Lucite International Diakon® CLG902L Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® Frost 902 51 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® Frost 952 51 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 180 MPa @Time 30.0 sec |
26100 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | ISO 2039-1 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Ball Indentation Hardness | 180 MPa @Load 98.0 kg, Time 30.0 sec |
26100 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 180 - 250 MPa | 26100 - 36300 psi | Average value: 205 MPa Grade Count:4 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Ball Indentation Hardness | 180 MPa | 26100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Ball Indentation Hardness | 180 MPa @Load 98.0 kg, Time 30.0 sec |
26100 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |