Nitriflex Nitrilatex NTL-218 Carboxylated Styrene Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name Nitrilatex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex Nitrilatex NTL-218 Carboxylated Styrene Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc. Information provided by Dax Resinas
Physical Properties Metric English Comments
Solids Content 48 - 50 %
48 - 50 %
Method L-001/P-065; ASTM D1417
pH 8.5 - 9.5
8.5 - 9.5
25°C, Method L-003; ASTM D1417
Brookfield Viscosity 90 - 200 cP
90 - 200 cP
(spindle=1, 20 rpm); ASTM D1417
Surface Tension 40 - 50 dynes/cm
40 - 50 dynes/cm
Method L-005/L-040; ASTM D1417