Polymer Property : Brookfield Viscosity = 90 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 90 - 200 cP
90 - 200 cP
(spindle=1, 20 rpm); ASTM D1417
Nitriflex Nitrilatex NTL-218 Carboxylated Styrene Butadiene Latex
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive..
Brookfield Viscosity 90 - 300 cP
90 - 300 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 6105 SBR Latex
ROVENE® 6105 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative low molecular weight and styrene content (45%) permits the formulation of pressure sensitive adhesi..