Nye Lubricants 350-SBG-2 (RL) Synthetic Oil

Category Fluid , Lubricant , Calcium Gellant , Organic Soap Gellant , White Mineral Oil (WMO)
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 350-SBG-2 (RL) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 61 cSt
61 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
Base Oil; ASTM D445
Evaporation Loss 1.0 %
1.0 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 280
280
ASTM D217
Oil Separation 10 %
10 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Recommended
Pour Point -21.0 °C
-5.80 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type WMO
Gellant Type Ca/Na soap