Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 176L (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 350-SBG-2 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Recommended |
Nye Lubricants 573H-40 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer A translucent beige compound with semi-crystalline perfluoropolymer nano-filler, specially developed to meet the demands of the semiconductor and bio-analytical industries. Compatible with fluorine .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70A Perfluoroelastomer A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G92A Perfluoroelastomer An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Origina.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V70J Fluoroelastomer Compound Grey Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z2, wher.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V70W Fluoroelastomer Compound Off-white Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z1,.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering V75L Fluoroelastomer Compound Special, steam-resistant Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1... |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to .. |
|||
Minimum Service Temperature, Air | -15.0 - 0.000 °C | 5.00 - 32.0 °F | Average value: -11.3 °C Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Freudenberg Simrit Simriz® 484 FDA FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Freudenberg Simrit Superiorâ„¢ F850 Fluoroelastomer Cost-effective, high performance compound for semiconductor applications. Superior F850 offers outstanding plasma resistance and low particulation in a wide range of plasma environments. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Freudenberg Simrit V141 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
GEHR Plastics PVC-ELS Polyvinylchloride, Electrically Conductive Grade Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Approx. Cold test |
Lubriplate 1241 Lithium-Polymer Type Multi-Purpose Grease Highly water resistant and tacky, they are designed for applications were the grease is subjected to heavy pressure and shock loads. This series is available in 3 NLGI densities for a wide range of .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B702 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ChevronTexaco Dura-Lith® NLGI 2 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ChevronTexaco NLGI 1 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Minimum Service Temperature, Air | -15.0 °C | 5.00 °F | Approx. Cold test |
Lubriplate 176 No. Inorganic/Organic Grease For Open Gearing This adhesive, semi-fluid grease is used for all types of open gears lubricated by centralized systems. Provides good pumpability without the use of harmful solvents. Applications: Open gears lubric.. |