Nye Lubricants 782KA (NG) Synthetic Oil

Category Fluid , Lubricant , Polyglycol , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 782KA (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 14 cSt
14 cSt
Base Oil; ASTM D445
Mechanical Properties Metric English Comments
Oil Separation 7.5 %
7.5 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Recommended
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Pour Point -37.0 °C
-34.6 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Polyglycol
Gellant Type Silica (WR)