Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended |
Nye Lubricants 570H-10 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | impact conditions and heavy loads not considered (dry sample) |
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | impact conditions and heavy loads not considered |
Omnia Plastica Omniamid PA6 GHR HR - Dry Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering E70D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 60-70 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering E70I Ethylene Propylene Rubber Resin cured Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated for applications involving water and steam.Applications: Recommended for us.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering Q70Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Precision Polymer Engineering Q90Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Radici Heraflex® P 40D 21 I HF Modified Polypropylene Shore hardness: 40D (3s)Shiny surface, very flexible even at very low T°C (to -30°C), good resistance to weather conditions, very light and recyclableApplication examples: low price, boots interna.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended |
Nye Lubricants 786A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering C90B Chloroprene Rubber Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Freudenberg Simrit Superiorâ„¢ F815 Fluoroelastomer Cost-effective, high performance compound for semiconductor applications. It offers outstanding plasma resistance and low particulation in a wide range of plasma environments. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Greene Tweed CHEMRAZ® 510 Perfluoroelastomer Greene Tweed’s Chemraz® 510, a perfluoroelastomer, offers an extremely broad range of chemical resistance with a Shore A hardness value of 90. with a temperature range form -22°F to 446Â.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer Chemraz® 585, a perfluoroelastomer, is a specialty cream compound formulated to outlast the most demanding chemical process applications. With its outstanding overall chemical resistance, Chemra.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance an.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucobit® 1233 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Recommended Operating Temperature |
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivit.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg B429 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg B747 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg Neoprene® C627 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Trelleborg Neoprene® C739 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | ASTM D 3575 |
Eurofoam Euroflex Art. 110 Polyurethane Foam Information provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
ChevronTexaco NLGI 2 SRI Grease FeaturesChevron SRI Grease is a high temperature ball and roller bearing grease.It is formulated with ISOSYN® base stocks, a synthetic polyurea ashless organic thickener, and high performance rust .. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Bostik 6327 Color Blending, Low Viscosity, Flexible EVA Glue Stick Bostik 6327 Color Blending, Low Viscosity, Flexible EVA Glue StickAdhesive color blends with substrate. Flexible, no cracking. Low viscosity. Easy to gun. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |
Bostik 6333 Medium Open Time, Low Viscosity, High Temp EVA Glue Stick Bostik 6333 Medium Open Time, Low Viscosity, High Temp EVA Glue StickMedium open time. Low viscosity. Easy to gun. Withstands elevated temperatures. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | ASTM D 3575 |
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |