Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 453 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry as molded. Injection molding grade. Nylene 453 is a UV stabilized, high viscosity nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance provided by 453 is attributed to highly uniform dispersion of 2% carbon black. With cylinder temperatures of 525 - 550ºF and mold temperatures of 140 - 160ºF, Nylene 453 can be molded into parts having a uniform, glossy appearance.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 191 °C
376 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
Users viewing this material also viewed the following: