Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | ASTM D648 |
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | ASTM D648 |
Nylene® 453 Nylon 6 Dry as molded. Injection molding grade. Nylene 453 is a UV stabilized, high viscosity nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance provided by 453 is a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | ASTM D648 |
Nylene® 453 Nylon 6, 50% RH Injection molding grade. Nylene 453 is a UV stabilized, high viscosity nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance provided by 453 is attributed to hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 375 °F | ASTM D648 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 375 °F | ASTM D648 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | |
Covestro Apec® DP 1-9379/7 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C @Thickness 3.20 mm |
376 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C @Thickness 3.20 mm |
376 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C @Thickness 3.20 mm |
376 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | ISO 75-1/-2 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 191 °C | 376 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 618 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |