Nylene® 7139 (HS) Low Wear Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 7139 (HS) Low Wear Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® 7139 (HS) is a general purpose, low wear, 1% MoS2 reinforced nylon 6/6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
490 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648