Material Notes:
Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll uniformity in cast film. In addition to a low coefficient of friction, it has excellent melt stability, high melt strength, and is gel free. Film from NX3055I has superior grease resistance, toughness, resistance to abrasion, and does not absorb food odors. Nylene NX3055I meets the requirements of FDA regulation 21 CFR 177.1500 for direct food contact. Optimum processing conditions should provide a melt temperature of 525 - 540ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 290 %
290 %
Orientation not specified; ASTM D882
Secant Modulus 0.650 GPa
94.3 ksi
ASTM D882
Elmendorf Tear Strength MD 56 g
56 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 60.0 MPa
8700 psi
Orientation not specified; ASTM D882
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F