Material Notes:
Description: Naxel™ PC506 is a 30% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Melt Flow 8.0 g/10 min
8.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 117 MPa
17000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
285 °F
ASTM D648