Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 20% Glass Filled
Manufacturer Nylene®
Trade Name Norpex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Norpex® AX20GF us a 20% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 96.5 MPa
14000 psi
ASTM D638
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
285 °F
ASTM D648
Users viewing this material also viewed the following: