Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether Description: Norpex® AX30GF is a 30% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Izod Impact, Notched | >= 1.12 J/cm | >= 2.10 ft-lb/in | ASTM D256 |
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-2102 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled
(discontinued **) Description/Features:30% Glass FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM Data |
Dow Questra® WA206 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2410R PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF30 TL5 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D 638 |
Styrolution PS 7120 HIPS Excellent ESCR to foodstuffs and PUR foamsGood low temperature impact strengthHigh relative stiffness/potential to down gauge sheetUL Classification 94 HBInformation provided by Styrolution |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 2510W Medium Impact Copolymer Polypropylene Impact CopolymerApplications: Trans-white battery casesFormolene 2510W is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dime.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ecomass® 1050TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ecomass® 1050ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 630-25G Nylon 6, 25% Glass Reinforced Nylon 6, 25% glass reinforced resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -40.0 °C |
2.10 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell ZR-17 33% Glass Reinforced Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general pu.. |
|||
Izod Impact, Notched | 1.12 J/cm @Diameter 3.17 mm |
2.10 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5711 High Impact Polystyrene
(discontinued **) High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF20 FR HS L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |