OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper

Category Metal , Metal Matrix Composite , Nonferrous Metal , Copper Alloy
Manufacturer OMG Americas
Trade Name GlidCop®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GlidCop® AL-25 is copper that is dispersion strengthened with 0.5 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum oxide is formed in the Cu matrix. The matrix is hardened while the Cu electrical and thermal conductivity are minimally lowered. The aluminum oxide particles are very thermally stable and remain effective in strengthening the copper matrix and resisting grain coarsening even after very long exposures to high temperatures as in brazing or high temp duty cycles.GlidCop® is available with three different levels of Al2O3. Increasing the Al2O3 levels will increase strength but decrease conductivities. All three grades can be further strengthened by cold work. GlidCop® is available in a wide range of extruded and drawn shapes and sizes, including rounds, rectangles, wire, plates, tubes, and strip. Available on a limited basis in powder form.Information provided by OMG Americas.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 296 - 372 MPa
42900 - 54000 psi
With 0% cold work
Thermal Properties Metric English Comments
Thermal Conductivity 344 W/m-K
2390 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Al2O3 0.50 %
0.50 %
Copper, Cu 99.5 %
99.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000200 ohm-cm
0.00000200 ohm-cm