Objet FullCure® 970 Tango Black Resin for Rapid Prototyping

Category Polymer , Rapid Prototyping Polymer
Manufacturer Objet
Trade Name FullCure®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Objet FullCure® 970 Tango Black Resin for Rapid Prototyping.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by American Precision Prototyping, LLC
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
ASTM D2240
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Elongation at Break 47.7 %
47.7 %
ASTM D412
Tear Strength 3.724 kN/m
21.25 pli
ASTM D624
Compression Set 0.80 %
0.80 %
ASTM D395
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -10.7 °C
12.7 °F
DSC (-80°C+100°C)