Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.00 MPa
290 psi
ISO 37
Multibase TPSiV® 4200-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Objet FullCure® 970 Tango Black Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer  (discontinued **)
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner ..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D638
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ISO 37
Kuraray SEPTON® S1001 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Momentive Performance Materials Silpruf® Construction Sealant
One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Momentive Performance Materials UltraPruf® SCS 2300 Construction Sealant
One-part, for concrete, masonry, and stone. Matte finish. Cure Method: Alkoxy (Neutral); Tack-free time 5 to 10 hr. Peel Strength 55 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE..
Tensile Strength, Ultimate 2.00 MPa
290 psi
ASTM D412
Momentive Performance Materials IGS3723 Insulating Glass Sealant
Two-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones becam..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Through Plane Direction
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Tensile Strength, Ultimate 2.00 MPa
290 psi
508 mm/min; ASTM D638
Dow Engage® 8130 Polyolefin Elastomer
Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process..
Tensile Strength, Ultimate 2.00 MPa
290 psi
508 mm/min; ASTM D638
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification...
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 141-55W185 Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and has physical..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo..
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-55W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall ..