Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Tris (chloroethyl) Phosphate (TCEP)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Tris (chloroethyl) Phosphate (TCEP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C6H12O4Cl3PCas No.: 29716-44-7Property: It is colorless or light yellow oily transparent liquid with slight cream odor. Soluble in common organic solvents, insoluble in aliphatic hydrocarbon, almost insoluble in water, good hydrolytic stability, slightly decomposed in alkaline solution, no obvious corrosiveness.Use: It has good performance for fire retarding and plasticity. It can be used as fire retardant for PVC, soft or hard foam polyurethane, cellulose acetate, ethyl cellulose paint, flame-resisting rubber and rubber conveyer belt. Besides self-extinguishing character, it can improve other performances of product, such as water proof, element resistance, antistatic performance, soft feeling, dosage is 5-10 portion, Ol. is 26. It can also be used as special pressure additives for lube, gasoline additives and heat cooling agent of magnesium.Storage and Packing: In galvanized metal pail. Storage temperature 5-38°C, not over 35°, in dry air. Common chemicals.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Specific Gravity 1.42 - 1.44 g/cc

@Temperature 204 °C
1.42 - 1.44 g/cc

@Temperature 399 °F
Viscosity 38 - 47 cP

@Temperature 20.0 °C
38 - 47 cP

@Temperature 68.0 °F
Molecular Weight 285.38 g/mol
285.38 g/mol
Thermal Properties Metric English Comments
Boiling Point 351 °C
664 °F
Decomposition Temperature 240 - 280 °C
464 - 536 °F
Flash Point 265.6 °C
510.1 °F
Optical Properties Metric English Comments
Refractive Index 1.47 - 1.479
1.47 - 1.479
n20D
Component Elements Properties Metric English Comments
Chlorine, Cl 37.3 %
37.3 %
Phosphorous, P 10.8 %
10.8 %
Descriptive Properties Value Comments
Acidity <0.20
mg KOH/g
Appearance Colorless or light yellow oily transparent liquid
CAS Number 29716-44-7
Chroma <100
Pt-Co
Molecular Formula C6H12O4Cl3P
Users viewing this material also viewed the following: