Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 38 - 47 cP @Temperature 20.0 °C |
38 - 47 cP @Temperature 68.0 °F |
|
Oceanchem Group Tris (chloroethyl) Phosphate (TCEP) Molecular Formula: C6H12O4Cl3PCas No.: 29716-44-7Property: It is colorless or light yellow oily transparent liquid with slight cream odor. Soluble in common organic solvents, insoluble in aliphatic.. |