Omni Plastics OmniLon™ 6 PA6 GR30 IM6 Glass Reinforced/Impact Modified Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Omni Plastics
Trade Name OmniLon™ 6
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniLon™ 6 PA6 GR30 IM6 Glass Reinforced/Impact Modified Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 MPa
21000 psi
ASTM D638
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256