Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.27 GPa | 1200 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 RM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Low Moisture Absorption and.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT (Asia Pacific) LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6 GF40 IM HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 0685 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHSL (DAM) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Ensinger Tecapeek® XP-119G Compression Molded PEEK Compound, 10% Carbon Fiber with 5% Graphite Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFN 6033 Glass Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 8.27 GPa @Temperature 149 °C |
1200 ksi @Temperature 300 °F |
ASTM D790 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF007 PA6.12 LNP THERMOCOMP* IF007 is a compound based on Nylon 6/12 resin containing 35% Glass Fiber. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton NV006E PC/ABS LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |