Material Notes:
A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Applications: Am ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated polyester compounds (BMC, SMC). Also used in paint applications, sealants, and adhesives.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Brightness 94 %
94 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.070 %
0.070 %
Moisture Loss at 110°C % (dry)
Particle Size 12 µm
12 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 97
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 0.5
Retained in 325 mesh (dry) ppm 0.2