Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 12 µm | 12 µm | median; Microtrac |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | >= 12 µm | >= 12 µm | 10% smaller than |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 12 µm | 12 µm | median; Microtrac |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 12 µm | >= 12 µm | 10% smaller than |
Nyco ULTRAFIBRE® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 12 µm | 12 µm | Median; Laser Diffraction |
Nabaltec APYMAG® 30S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Particle Size | 12 µm | 12 µm | Median Grain Diameter |
Nabaltec APYRAL® 4 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 12 µm | 12 µm | Median Diameter |
Omya OMYACARB® 10 - LU Calcium Carbonate A medium, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 17-7 PH Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 316L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 317L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 4140 Low Alloy Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 4340 Low Alloy Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 85/15 Cu Sn Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Co212-e Cobalt Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals M2 Tool Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals S2 Tool Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 17-4 PH Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Material Notes: Composition above is typical of.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 434L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 80/20 Ni Cr Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Fe30Cr Binary Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | mean |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Particle Size | 12 µm | 12 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 12 µm | 12 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline A-6209 A-6209 is a standard grade; class "B", medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance |
|||
Particle Size | 12 µm | 12 µm | |
Shin-Etsu Silicones KSP-101 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline StarBrite® 3102 These Vacuum Metallized Flake (VMF) pigments are extremely thin, non-leafing, lamellar aluminum pigments. These exacting characteristics allow the formulator to achieve a smooth, mirror-like metall.. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline StarBrite® 4102 These Vacuum Metallized Flake (VMF) pigments are extremely thin, non-leafing, lamellar aluminum pigments. These exacting characteristics allow the formulator to achieve a smooth, mirror-like metall.. |
|||
Particle Size | <= 12 µm | <= 12 µm | Max |
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan Elite and BariScan Ultra barite meet and exceed the requ.. |
|||
Particle Size | 12 µm | 12 µm | 10th% |
3M iM16K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |