Omya OMYACARB® 6 - PT Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYACARB®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYACARB® 6 - PT Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A dry ground calcium carbonate with intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated polyester compounds (SMC, BMC, TMC). Also used in paint applications.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.71 g/cc
2.71 g/cc
Bulk Density 1.35 g/cc
0.0488 lb/in³
Packed
Brightness 95 %
95 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.050 %
0.050 %
Moisture Loss at 110°C % (dry)
Particle Size 6.0 µm
6.0 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 96
DOP Absorption, g DOP/100 g pigment 19.5
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 9.5
Magnesium Carbonate % 2
Retained in 325 mesh (dry) ppm 0.03
Users viewing this material also viewed the following: