Omya OMYACARB® BP - AZ Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYACARB®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYACARB® BP - AZ Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A dry ground calcium carbonate with a medium and closely sized particle distribution and excellent shrink resistance properties.Applications: Ideal for joint compounds, unsaturated polyester, cementitious grouts and plasters, plastics, and adhesives.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Brightness 93 %
93 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.020 %
0.020 %
Moisture Loss at 110°C % (dry)
Particle Size 20 µm
20 µm
Median Diameter
Descriptive Properties Value Comments
Calcium Carbonate % 97
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 0.5
Retained in 100 mesh, (dry) % 0.001
Retained in 325 mesh (dry) ppm 9