Omya OMYAFLOW® 3 - SY Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYAFLOW®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYAFLOW® 3 - SY Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Decorative paints.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 1.83 g/cc
1.83 g/cc
Density 1.83 g/cc
0.0662 lb/in³
Slurry
Solids Content 72 %
72 %
as Supplied
Brightness 98 %
98 %
Y - Brightness (dry)
Particle Size 3.2 µm
3.2 µm
Median Diameter
Specific Surface Area 3.2 m²/g
3.2 m²/g
Brookfield Viscosity 140 cP

@Temperature 25.0 °C
140 cP

@Temperature 77.0 °F
No. 3 Spindle, 100 rpm
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 1
Pounds Pigment/gallon (slurry) 11.01
Pounds Pigment/Solid Gallon (dry) 11.01
Retained in 325 mesh (dry) ppm 3