Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.2 µm | 3.2 µm | Median Diameter |
Omya HYDROCARB® PG-3 Calcium Carbonate A ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Particle Size | 3.2 µm | 3.2 µm | Median Diameter |
Omya OMYACARB® 3 - FL Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Employed in rubber and plastic applications such as ri.. |
|||
Particle Size | 3.2 µm | 3.2 µm | Median Diameter |
Omya OMYAFLOW® 3 - SY Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Decorative paints.Information supplied by Omya North A.. |
|||
Particle Size | 3.2 µm | 3.2 µm | Median Diameter |
Omya SNOWHITE® 3 - PT Calcium Carbonate A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics.Applications: Employed in rubber and plastic applications such as rigid PVC and plasticized PVC. Also us.. |