Omya OMYAPAQUE® Calcium Carbonate

Category Ceramic
Manufacturer Omya North America
Trade Name OMYAPAQUE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYAPAQUE® Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An ultrafine ground calcium carbonate for paper and board filling. An opacifying product that is designed to reduce costs through the replacement of more expensive pigments.Information supplied by Omya North America.
Physical Properties Metric English Comments
Solids Content 63 %
63 %
Slurry Solids
Brightness 96 %
96 %
T534 om-76 Brightness (Diffuse Reflectance)
Loss On Ignition 0.000 %

@Temperature 400 °C
0.000 %

@Temperature 752 °F
42.6 %

@Temperature 900 °C
42.6 %

@Temperature 1650 °F
Particle Size 0.80 µm
0.80 µm
Median Diameter
Specific Surface Area 8.0 m²/g
8.0 m²/g
Brookfield Viscosity 300 cP

@Temperature 25.0 °C
300 cP

@Temperature 77.0 °F
No. 3 Spindle, 100 rpm
Optical Properties Metric English Comments
Reflection Coefficient, Visible (0-1) 0.96
0.96
T534 om-76 Brightness (Diffuse Reflectance)
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 176.170, 176.180
Magnesium Carbonate % 1