Outokumpu 304 PRODEC® Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Outokumpu
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Outokumpu 304 PRODEC® Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Outokumpu branded grade, offering significantly improved machinability due to special steel making practice and chemistry.Information provided by Outo Kumpu
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 18.3 %
18.3 %
Iron, Fe 72.42 %
72.42 %
Nickel, Ni 9.2 %
9.2 %
Nitrogen, N 0.060 %
0.060 %