Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Nima™ NH PC143P Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name Nima™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nima™ NH PC143P Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-Hal FR-PC with High impact and improved processabilityAll properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
50 mm/min; ASTM D638
Elongation at Break 40 %
40 %
50 mm/min; ASTM D638
Tensile Modulus 1.60 GPa
232 ksi
50 mm/min; ASTM D638
Flexural Strength 70.0 MPa
10200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.50 J/cm

@Temperature -30.0 °C
2.81 ft-lb/in

@Temperature -22.0 °F
ASTM D256
7.31 J/cm

@Temperature 23.0 °C
13.7 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C

@Thickness 3.20 mm
248 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94 V-0